Gunite vs Shotcrete: How Concrete Pools Are Actually Built

Table of Contents

What you need to know in 30 seconds

  • Gunite and shotcrete aren’t two materials: both spray concrete at high speed, and gunite is the dry-mix version.
  • With gunite, water is added at the nozzle; with wet-mix shotcrete, the concrete arrives premixed from a ready-mix truck.
  • The American Shotcrete Association says both methods produce strong, watertight shells when a skilled crew does the work.
  • A concrete pool is built in layers: excavation, a rebar cage, the sprayed shell, a bond beam, curing, and a plaster or pebble finish.

Nozzle operator spraying concrete over a steel rebar cage inside an excavated backyard pool

Gunite vs shotcrete is one of the most argued topics in pool building, and most of the argument is about a name. Both are pneumatically applied concrete: concrete shot from a hose at high speed so the impact packs it tight.

Full disclosure: we install Latham fiberglass pools, not concrete, so we have no horse in this race. Our take: if you choose concrete, judge the builder’s curing plan before the spray method.

The short answer: gunite is dry-mix shotcrete, where water joins the dry cement and sand at the nozzle. Shotcrete usually means wet-mix, where premixed concrete is pumped and shot. According to the American Shotcrete Association, both build strong, watertight pool shells when placed correctly by an experienced crew.

 

What is the difference between gunite and shotcrete?

Diagram comparing dry-mix gunite, with water added at the nozzle, and wet-mix shotcrete pumped from a ready-mix truck

The difference between gunite and shotcrete is when water meets the cement. In a 2018 Shotcrete magazine article, the American Shotcrete Association (ASA) explains that both are placement methods, not materials.

“Gunite” began as the Cement Gun Company’s trade name for its dry process. In 1951 the American Concrete Institute adopted the neutral term “shotcrete,” covering all pneumatically applied concrete, later split into wet-mix and dry-mix.

Think of pancake batter: wet-mix arrives already stirred, while dry-mix is flour that meets water the instant it leaves the spout.

How does gunite (dry-mix) work?

Close-up of a nozzle operator's hand adjusting the water valve on a dry-mix gunite hose

Gunite blows dry cement and sand through a hose, and the nozzle operator adds water at the tip. That live control is both its strength and its risk.

The ASA puts typical dry-mix water-to-cement ratios at 0.35 to 0.40. Less water usually means less shrinkage, if the operator holds it steady.

How does wet-mix shotcrete work?

Ready-mix concrete truck feeding a concrete pump parked beside a backyard pool excavation

Wet-mix shotcrete pumps premixed concrete from a ready-mix truck and air shoots it into place. The ASA puts its typical ratio at 0.40 to 0.45.

The weak point is the jobsite: the ASA warns crews often add water to a stiffening load, pushing the ratio past 0.50 and weakening the shell.

Is gunite or shotcrete stronger?

Row of concrete test cylinders beside a compression testing machine in a materials lab

Neither is automatically stronger. The ASA says both produce strong, functionally impermeable shells with the right mix.

What does matter is the number. ASA’s Position Statement #1 sets a 4,000 psi minimum in-place compressive strength for pool shotcrete, citing ACI 318 requirements for concrete in contact with water.

Factor Gunite (dry-mix) Shotcrete (wet-mix)
Water added At the nozzle At the plant
Typical water-to-cement ratio 0.35 to 0.40 0.40 to 0.45
Who controls the mix Nozzle operator, live Batch plant, then crew
Main risk Inconsistent water at the nozzle Extra water added on site
Strength with correct mix 4,000 psi minimum per ASA 4,000 psi minimum per ASA

 

How are concrete pools built, step by step?

Aerial view of a backyard concrete pool under construction with excavation, rebar, and forms in place

Here’s how concrete pools are built, in the order a typical crew works:

  1. Excavate and form the hole and its top edge.
  2. Rough in plumbing for drains, returns, and skimmers.
  3. Tie the rebar cage to follow every curve.
  4. Shoot the shell with gunite or shotcrete.
  5. Shape the bond beam to carry coping and deck.
  6. Cure the shell by keeping it wet.
  7. Add tile, coping, and decking.
  8. Apply the finish: plaster, quartz, or pebble.

What does a rebar cage do in a pool?

Tied steel rebar grid lining a curved pool excavation, raised off the soil on small concrete blocks

A rebar cage is the steel grid that gives a concrete pool tensile strength. Concrete resists crushing but cracks under bending, so rebar takes the pull.

Picture a skyscraper’s steel frame wrapped in concrete. The cage must sit off the soil so concrete fully surrounds it, and the ASA lists inadequate rebar among common causes of cracked shells.

Why does shotcrete pool construction need high velocity?

Stream of sprayed concrete striking a pool wall at speed, with loose rebound material falling to the floor

Shotcrete pool construction depends on speed, because impact is what compacts pneumatically applied concrete. In an ASA technical column, Charles Hanskat notes that the material typically strikes at 50 to 80 mph.

Material that bounces off, called rebound, is mostly sand and rock. The ASA says it must be removed, not buried in floors and benches.

The shell should also be one continuous piece. ASA’s Position Statement #5 calls for monolithic shells with no cold joints, the weak seams left when fresh concrete meets hardened concrete.

What is a pool bond beam?

Thick concrete top edge of a new pool shell, ready to receive coping stones and decking

A bond beam is the thickened, steel-reinforced top edge of the shell. It ties the walls together and carries the coping, the edge stones you sit on.

It works like a bucket’s rim: without it, the walls flex. Fiberglass pools use one too, as our fiberglass pool installation process covers.

Why does curing matter more than the spray method?

Worker hosing down a fresh gray concrete pool shell to keep it wet on a hot, sunny day

Curing matters because concrete gains strength through hydration, a chemical reaction between Portland cement and water. If the surface dries out early, that reaction stops at the surface.

ASA’s Position Statement #7 on curing pools says about 70% of cement hydration happens in the first 7 days. ACI and ASA typically require curing for at least 7 days.

Stretching wet curing from 3 to 7 days can cut surface shrinkage cracking by 10% to 20%. Before plaster, ACI Committee 524 and the National Plasterers Council recommend 28 days of moist curing.

That’s where Central Texas heat bites. Hanskat describes an Arizona pool that cracked despite twice-daily watering; hot, dry wind demands continuous moisture.

What is pool plaster? Pool plaster explained

Plaster crew wearing spiked shoes troweling a smooth white finish onto a drained concrete pool shell

Here’s pool plaster explained simply: it’s the thin, waterproof interior finish troweled over the concrete shell. The American Concrete Institute’s pool plastering technote, ACI 524.1-24, calls it a nonstructural cementitious finish of white cement and aggregate.

Plaster is the skin, not the skeleton. The shell carries the load; plaster seals and colors the surface. A badly cured shell can undermine even a perfect plaster job.

What is a pebble finish?

Close-up of a pebble pool finish showing small rounded blue and gray stones set in cement

A pebble finish is a plaster that uses small, rounded stones as the aggregate instead of marble dust. ACI 524.1-24 notes that combining white cement and pigment with different colored aggregates produces a wide range of finishes.

The result has a more textured feel underfoot than standard white plaster. Our gel coat vs plaster guide compares these surfaces with a fiberglass pool’s finish.

Should you choose gunite, shotcrete, or a different pool type?

Choose the crew, not the acronym. Prioritize gunite if your builder’s operators know dry-mix well; prioritize wet-mix if they run tight ready-mix schedules and use water-reducing admixtures instead of added water.

Ask any concrete builder these questions:

  • What compressive strength do you specify? At least 4,000 psi, per the ASA.
  • Do you remove rebound? The answer should be yes, every time.
  • How long do you wet cure, and how often? Seven days minimum; 28 before plaster is ideal.
  • Who certifies your nozzle operators? ACI offers nozzleman certification.

If concrete’s timeline and upkeep give you pause, our fiberglass vs concrete pool comparison lays out the tradeoffs. You can also request a free quote for a Latham fiberglass pool.

Frequently asked questions

Is a gunite pool the same as a concrete pool?

Cross-section diagram of a concrete pool wall showing soil, rebar, sprayed shell, and plaster layers

Yes. A gunite pool is a concrete pool whose shell was sprayed with the dry-mix method. “Shotcrete pool” usually means the wet-mix method. Both end up as rebar-reinforced concrete shells finished with plaster or pebble.

How long does it take to build a concrete pool?

Most concrete pools take months, not weeks. Shooting the shell takes a day or two, but curing, tile, decking, and plastering stretch the schedule. Our types of swimming pools guide compares build times across pool types.

Why do concrete pool shells crack?

Hairline crack running across a gray concrete pool shell before the plaster is applied

The ASA lists common causes as inadequate rebar, poor soil, poor curing, seasonal temperature swings, concrete shrinkage, and rebound left in the shell. Most cracks have nothing to do with gunite vs shotcrete itself.

The bottom line on gunite vs shotcrete

Gunite and shotcrete are two ways to spray the same thing: Portland cement concrete wrapped around a rebar cage. A skilled crew, a 4,000 psi mix, rebound removal, and patient curing decide whether a shell lasts.

Still weighing pool types? Read our things to know before building a pool, or call (254) 855-5616.

Get Your Free Quote

Meet Our Expert
Marvin Dueck

Marvin Dueck

Pool Installation Specialist

Pool installation specialist at Backyard Boyz Texas, helping Central Texas homeowners design and build durable, low-maintenance fiberglass pools.

Get Started Today

Fill out the form below, and our local team will reach out shortly.

The Steps

The Process Is Easy!

Short Loan Application

It won't hurt your credit!
A soft credit check helps us have a meaningful conversation about your personal needs and qualifications.

Personal Consultation

You'll meet with your personal pool loan consultant to review your options and select the best loan option for you. There is no obligation.

Fast Loan Process

We work together to quickly process your loan and get an approval decision. We keep you informed every step of the way.

Loan Funding

High approval rates for a wide range of credit profiles. Fund disbursements vary by loan option. Your Loan Consultant will explain all the details.

No obligation. Soft credit check only.